ASTM A513 Type 1 ERW Carbon Steel Pipe is a straight seam electric resistance welded (ERW) carbon steel pipe produced in accordance with ASTM A513 standard.
Wyślij zapytanie
Czatuj teraz
Wprowadzenie produktów

ASTM A513 Type 1 Straight Seam Welded Pipe, and we provide high-quality steel pipes to customers all over the world based on their needs.

Compared to A5131B steel pipe, ASTM A513 1A mechanical pipe is made from hot-rolled steel strips that are pickled to remove the oxide scale and then oiled to provide a cleaner surface than the hot-rolled surface. A513 Type 1 mechanical pipe is generally used in applications that require bending, flanging, flaring, or flattening.
With excellent weldability, formability, and corrosion resistance, A513 Type 1 welded pipe is used in a variety of industries, including automotive, construction, and industrial equipment.

sales@gneetube.com
 

ASTM A513 tshuaj lom neeg muaj pes tsawg leeg :

1010

0.05-0.15

0.30-0.60

0.035

0.035

1015

0.10-0.20

0.30-0.60

0.035

0.035

1020

0.15-0.25

0.30-0.60

0.035

0.035

1026

0.22-0.28

0.60-0.90

0.035

0.035

ASTM A513 khoom siv lub cev :

Elongation hauv 2 hauv. Lossis 50 hli. % kwv

1008

30 (207)

42 (290)

15 15

1010

32 (221)

45 (310)

15 15

1015

35 (241)

48 (331)

15 15

1020

38 (262) |

52 (359)

12. 12s

1026

45 (310)

62 (427)

12. 12s

ASTM A513 Carbon Steel Mechanical Tubing

ASTM A513 hydraulic pipes

 

Gnee company covers an area of 35,000 square meters and has more than 200 employees, including 80 technical staff. We have established an effective and complete quality control and assurance system. The company has also obtained ISO9001 quality system certification.

ASTM A513 Type 1 Tubing

1. Strong stainless steel production capacity, technology and quality control system.
2. Evaluate suppliers and credit companies.
3. A foreign trade sales team with professional services and a high reputation in overseas markets.
4. The core team has more than 10 years of experience in steel pipe foreign trade business to ensure that your order is worry-free.

Popularne Tagi: astm a513 type 1 tubing, China astm a513 type 1 tubing manufacturers, suppliers, factory, Spawana rura stalowa do energii słonecznej

Wyślij zapytanie

whatsapp

Telefon

Adres e-mail

Zapytanie